Ore Mining Process With Cencentrating Products High Efficient
Concentrating. The ore is enriched using a process called froth flotation. Unwanted material called gangue sinks to the bottom and is removed. Roasting. This is where the chemical reactions start. The powdered, enriched ore is heated in air between 500176C and 700176C to remove some sulphur and dry the ore, which is still a solid called calcine.